Causes and solutions of blowholes in die-casting parts

  • Categories:News
  • Author:
  • Origin:
  • Time of issue:2020-10-30 16:25
  • Views:

(Summary description)Zinc die-casting is a casting in which zinc liquid is quickly and high-pressure filled into the mold cavity. The time for zinc liquid to fill the die-casting cavity is extremely short, generally a few hundredths of a second or a few thousandths of a second. The pores formed during the die casting process have a smooth surface...

Causes and solutions of blowholes in die-casting parts

(Summary description)Zinc die-casting is a casting in which zinc liquid is quickly and high-pressure filled into the mold cavity. The time for zinc liquid to fill the die-casting cavity is extremely short, generally a few hundredths of a second or a few thousandths of a second. The pores formed during the die casting process have a smooth surface...

  • Categories:News
  • Author:
  • Origin:
  • Time of issue:2020-10-30 16:25
  • Views:
Information

Zinc die-casting is a casting in which zinc liquid is quickly and high-pressure filled into the mold cavity. The time for zinc liquid to fill the die-casting cavity is extremely short, generally a few hundredths of a second or a few thousandths of a second. The pores formed during the die casting process have a smooth surface...

Scan the QR code to read on your phone

底部logo

Ningbo Xinghuang Photoelectricity Co.,Ltd

CONTANT US

 

Tel:86-574-62250222

 

Phone:86-13505847262

 

E-mail:cyf@zjxhgd.com

 

Add:Huangqingyan Village Ditang Town Yuyao ,Zhejiang , China

搜索
Search

Insist on doing things right the first time and try our best to provide customers with perfect products and services.

Copyrights© 2021 Ningbo Xinghuang Photoelectricity Co.,Ltd 版权所有 浙ICP备05056522号-1  Website construction:www.300.cn Ningbo